MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C70400, H02 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot formability. Fabricated by forming, bending and welding.

Applications: condensers, evaporators, heat exchangers, ferrules, salt water piping, lithium bromide absorption tubing, shipboard condenser intake systems.

Available as flat products and tube.

Key Words: CDA 704 (95/5)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 6767
Hardness, Rockwell 30T 6565
Tensile Strength, Ultimate 395 MPa57300 psi
Tensile Strength, Yield 380 MPa
@Strain 0.2 %
55100 psi
@Strain 0.2 %
Elongation at Break 11 %11 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.310.31Calculated
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000120 ohm-cm
@Temperature 20.0 °C
0.0000120 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.5 µm/m-°C
@Temperature 20.0 - 300 °C
9.72 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 64.0 W/m-K
@Temperature 20.0 °C
444 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1125 °C<= 2057 °F
Liquidus 1125 °C2057 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 565 - 815 °C1050 - 1500 °F
Hot-Working Temperature 815 - 950 °C1500 - 1740 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 91.2 %>= 91.2 %
Iron, Fe 1.3 - 1.7 %1.3 - 1.7 %
Lead, Pb <= 0.050 %<= 0.050 %
Manganese, Mn 0.30 - 0.80 %0.30 - 0.80 %
Nickel, Ni 4.8 - 6.2 %4.8 - 6.2 %
Zinc, Zn <= 1.0 %<= 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C41100, H03 Temper flat products
Copper, UNS C41100, H02 Temper flat products
Copper, UNS C19700, H04 Temper
Commercial Bronze, UNS C22000 (90-10 Bronze), H04 Temper flat products
Chromium Copper, UNS C18400, TD04 Temper flat products

MC70400b5 / 11712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.