MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pressure Seal 9703 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 9703 is a 75 durometer purple colored Fluorinated Hydrocarbon elastomer. It is specifically formulated for low temperature applications. It also exhibits good resistance to compression set, petroleum based oils, aliphatic and aromatic fuels and oxygenated fuels.

This compound will meet or exceed the specifications listed and has the following physical properties: ALL TEST RESULTS ARE ON AS 568 -214 O-RINGS
This Compound is RoHS Compliant

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.07 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77
 72
@Treatment Temp. 23.0 °C,
Time 252000 sec
Methanol
 74
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 75
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 76
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 77
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1326 psi
 844.7 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
Methanol
 934.8 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 936.2 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 1225.2 psi
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 1470.5 psi
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 109 %
 91.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel B
 93.3 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel C
 93.3 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Methanol
 116.6 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
ASTM Reference Fuel A
 172 %
@Treatment Temp. 250 °C,
Time 252000 sec
Heat Aged
100% Modulus 1227 psi
Compression Set 8.0 %
@Treatment Temp. 175 °C,
Time 79200 sec
O-Ring
 13.6 %
@Treatment Temp. 200 °C,
Time 79200 sec
O-Ring
 14.7 %
@Treatment Temp. 200 °C,
Time 252000 sec
O-Ring
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -49.0 °F
Shrinkage 1.1 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel A
 3.9 %
@Treatment Temp. 23.0 °C,
Time 6.84e+6 sec
Volume, ASTM Reference Fuel A
 4.0 %
@Treatment Temp. 23.0 °C,
Time 1.01e+7 sec
Volume, ASTM Reference Fuel A
 4.6 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel B
 6.5 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, ASTM Reference Fuel C
 7.3 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
Volume, Methanol
 8.7 %
@Treatment Temp. 23.0 °C,
Time 6.84e+6 sec
Volume, ASTM Reference Fuel B
 8.7 %
@Treatment Temp. 23.0 °C,
Time 1.01e+7 sec
Volume, ASTM Reference Fuel B
 10.3 %
@Treatment Temp. 23.0 °C,
Time 6.84e+6 sec
Volume, ASTM Reference Fuel C
 10.3 %
@Treatment Temp. 23.0 °C,
Time 1.01e+7 sec
Volume, ASTM Reference Fuel C
 11.9 %
@Treatment Temp. 23.0 °C,
Time 6.84e+6 sec
Volume, 15% EtOH/85% FUEL C
 12.4 %
@Treatment Temp. 23.0 °C,
Time 1.01e+7 sec
Volume, 15% EtOH/85% FUEL C
 13.5 %
@Treatment Temp. 23.0 °C,
Time 6.84e+6 sec
Volume, Methanol
 13.9 %
@Treatment Temp. 23.0 °C,
Time 1.01e+7 sec
Volume, Methanol
 
Descriptive Properties
ColorPurple
TR-10 Temperature-40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL115 / 318325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.