Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 2.07 g/cc | 2.07 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 77 | 77 |
| 72 @Treatment Temp. 23.0 °C, Time 252000 sec | 72 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 74 @Treatment Temp. 23.0 °C, Time 252000 sec | 74 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 75 @Treatment Temp. 23.0 °C, Time 252000 sec | 75 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 76 @Treatment Temp. 23.0 °C, Time 252000 sec | 76 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 77 @Treatment Temp. 250 °C, Time 252000 sec | 77 @Treatment Temp. 482 °F, Time 70.0 hour |
Tensile Strength | 9.142 MPa | 1326 psi |
| 5.824 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 844.7 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 6.445 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 934.8 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 6.455 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 936.2 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 8.4475 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1225.2 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 10.139 MPa @Treatment Temp. 250 °C, Time 252000 sec | 1470.5 psi @Treatment Temp. 482 °F, Time 70.0 hour |
Elongation, Ultimate | 109 % | 109 % |
| 91.5 % @Treatment Temp. 23.0 °C, Time 252000 sec | 91.5 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 93.3 % @Treatment Temp. 23.0 °C, Time 252000 sec | 93.3 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 93.3 % @Treatment Temp. 23.0 °C, Time 252000 sec | 93.3 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 116.6 % @Treatment Temp. 23.0 °C, Time 252000 sec | 116.6 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 172 % @Treatment Temp. 250 °C, Time 252000 sec | 172 % @Treatment Temp. 482 °F, Time 70.0 hour |
100% Modulus | 8.460 MPa | 1227 psi |
Compression Set | 8.0 % @Treatment Temp. 175 °C, Time 79200 sec | 8.0 % @Treatment Temp. 347 °F, Time 22.0 hour |
| 13.6 % @Treatment Temp. 200 °C, Time 79200 sec | 13.6 % @Treatment Temp. 392 °F, Time 22.0 hour |
| 14.7 % @Treatment Temp. 200 °C, Time 252000 sec | 14.7 % @Treatment Temp. 392 °F, Time 70.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -45.0 °C | -49.0 °F |
Shrinkage | 1.1 % @Treatment Temp. 23.0 °C, Time 252000 sec | 1.1 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 3.9 % @Treatment Temp. 23.0 °C, Time 6.84e+6 sec | 3.9 % @Treatment Temp. 73.4 °F, Time 1900 hour |
| 4.0 % @Treatment Temp. 23.0 °C, Time 1.01e+7 sec | 4.0 % @Treatment Temp. 73.4 °F, Time 2800 hour |
| 4.6 % @Treatment Temp. 23.0 °C, Time 252000 sec | 4.6 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 6.5 % @Treatment Temp. 23.0 °C, Time 252000 sec | 6.5 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 7.3 % @Treatment Temp. 23.0 °C, Time 252000 sec | 7.3 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 8.7 % @Treatment Temp. 23.0 °C, Time 6.84e+6 sec | 8.7 % @Treatment Temp. 73.4 °F, Time 1900 hour |
| 8.7 % @Treatment Temp. 23.0 °C, Time 1.01e+7 sec | 8.7 % @Treatment Temp. 73.4 °F, Time 2800 hour |
| 10.3 % @Treatment Temp. 23.0 °C, Time 6.84e+6 sec | 10.3 % @Treatment Temp. 73.4 °F, Time 1900 hour |
| 10.3 % @Treatment Temp. 23.0 °C, Time 1.01e+7 sec | 10.3 % @Treatment Temp. 73.4 °F, Time 2800 hour |
| 11.9 % @Treatment Temp. 23.0 °C, Time 6.84e+6 sec | 11.9 % @Treatment Temp. 73.4 °F, Time 1900 hour |
| 12.4 % @Treatment Temp. 23.0 °C, Time 1.01e+7 sec | 12.4 % @Treatment Temp. 73.4 °F, Time 2800 hour |
| 13.5 % @Treatment Temp. 23.0 °C, Time 6.84e+6 sec | 13.5 % @Treatment Temp. 73.4 °F, Time 1900 hour |
| 13.9 % @Treatment Temp. 23.0 °C, Time 1.01e+7 sec | 13.9 % @Treatment Temp. 73.4 °F, Time 2800 hour |
|
Descriptive Properties |
---|
Color | Purple |
TR-10 Temperature | -40°C |