MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Data provided by Carpenter Technology Corporation.

Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.

Gall-Tough® stainless is a high silicon, high manganese, nitrogen strengthened, austenitic stainless alloy which possesses superior self-mated galling resistance and metal-to-metal wear resistance. The alloy possesses higher strength and high temperature oxidation resistance than Type 304 stainless with comparable corrosion resistance, depending on the environment.

Gall-Tough® is a registered trademark of Carpenter Technology Corporation.

Key Words: ASTM A479; ASTM A276; ASTM A314; ASTM A580; ASTM A240
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 979 MPa
 1344 MPa
@Temperature -73.0 °C
Tensile Strength, Yield 379 MPa
@Strain 0.2 %
 448 MPa
@Strain 0.2 %,
Temperature -73.0 °C
Elongation at Break 59 %in 4D
 47 %
@Temperature -73.0 °C
in 4D
Reduction of Area 59 %
 68 %
@Temperature -73.0 °C
Modulus of Elasticity 171.1 GPa
@Temperature 23.0 °C
Charpy Impact 325 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000716 ohm-cm
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.3 µm/m-°C
@Temperature 25.0 - 100 °C
 17.73 µm/m-°C
@Temperature 25.0 - 250 °C
 18.5 µm/m-°C
@Temperature 25.0 - 500 °C
Specific Heat Capacity 0.5145 J/g-°C
@Temperature 52.0 - 102 °C
Thermal Conductivity 12.22 W/m-K
@Temperature 23.0 °C
Maximum Service Temperature, Air 982 °CScaling Temperature for Continuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 15 - 18 %
Iron, Fe 68 %as remainder
Manganese, Mn 4.0 - 6.0 %
Molybdenum, Mo 0.50 - 2.5 %
Nickel, Ni 4.0 - 6.0 %
Nitrogen, N 0.080 - 0.20 %
Phosphorus, P <= 0.040 %
Silicon, Si 3.0 - 4.0 %
Sulfur, S <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work
ATI Allegheny Ludlum Stainless Steel Type 301, 1/2 Hard (UNS S30100)
Carpenter Gall-Tough® Stainless
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Longitudinal Properties
Carpenter Pyrowear® 675 Stainless Steel, Tempered 316°C, Transverse Properties

NCAR2B / 15614

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.