MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals NIMONIC® Alloy 86
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A nickel-chromium-molybdenum alloy with a rare-earth (cerium) addition. It combines good formability and weldability with exceptional resistance to oxidation and scaling at temperatures to 1920°F (1050°C). Used in gas turbines for sheet-metal fabrications such as combustion chambers and afterburners and in heat-treating furnaces. Standard product forms are round, extruded section, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 MPa
@Temperature 650 °C
Solution Annealed prior to test
 825 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 410 MPa
@Strain 0.2 %
Solution Annealed. Value at room temperature
 240 MPa
@Strain 0.2 %,
Temperature 650 °C
Solution Annealed prior to test
Elongation at Break 42 %Solution Annealed
 50 %
@Temperature 650 °C
Solution Annealed prior to test.
Modulus of Elasticity 210 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.7 µm/m-°C
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.050 %
Cerium, Ce 0.030 %
Chromium, Cr 25 %
Molybdenum, Mo 10 %
Nickel, Ni 65 %As remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals NIMONIC® Alloy 81
Special Metals NIMONIC® Alloy 105
Special Metals NIMONIC® Alloy 115
Special Metals NIMONIC® Alloy 263
Special Metals NIMONIC® Alloy 75

NINC63 / 17413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.