MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Special Metals NIMONIC® Alloy 81
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A precipitation-hardenable nickel-chromium alloy with enhanced resistance to high-temperature corrosion. The excellent hot-corrosion resistance of the alloy results from its high chromium content of 30%. The alloy also has good tensile and rupture strength and creep resistance at elevated temperatures. Used for gas turbines, piston-engine exhaust valves, and furnace equipment subject to attack by deposits resulting from combustion of impure fuels, particularly those containing alkali metal sulfates and chlorides. The standard product form is round.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.06 g/cc0.291 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  830 MPa
@Temperature 650 °C
120000 psi
@Temperature 1200 °F
Precipitation Hardened prior to test
 1050 MPa
@Temperature 23.0 °C
152000 psi
@Temperature 73.4 °F
Tensile Strength, Yield 600 MPa
@Strain 0.2 %
87000 psi
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 520 MPa
@Strain 0.2 %,
Temperature 650 °C
75400 psi
@Strain 0.2 %,
Temperature 1200 °F
Precipitation Hardened prior to test
Elongation at Break 40 %40 %Precipitation Hardened
 30 %
@Temperature 650 °C
30 %
@Temperature 1200 °F
Precipitation Hardened prior to test.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000127 ohm-cm0.000127 ohm-cm
Magnetic Permeability 1.00041.0004at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesMetricEnglishComments
CTE, linear 11.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.17 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.461 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 10.9 W/m-K75.6 BTU-in/hr-ft²-°F
Melting Point 1305 - 1375 °C2381 - 2507 °F
Solidus 1305 °C2381 °F
Liquidus 1375 °C2507 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.90 %0.90 %
Boron, B 0.0030 %0.0030 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr <= 30 %<= 30 %
Cobalt, Co <= 2.0 %<= 2.0 %
Copper, Cu <= 0.20 %<= 0.20 %
Iron, Fe <= 1.0 %<= 1.0 %
Manganese, Mn <= 0.50 %<= 0.50 %
Molybdenum, Mo <= 0.30 %<= 0.30 %
Nickel, Ni 63 %63 %As remainder
Silicon, Si <= 0.50 %<= 0.50 %
Sulfur, S <= 0.015 %<= 0.015 %
Titanium, Ti 1.8 %1.8 %
Zirconium, Zr 0.060 %0.060 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals NIMONIC® Alloy 80A
Special Metals NIMONIC® Alloy 263
Special Metals NIMONIC® Alloy 86
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy
Special Metals NIMONIC® Alloy 105

NINC62 / 17412

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.