MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ThyssenKrupp N-A-XTRA® 620 Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield strength of 550, 620 and 700 MPa. All steel grades can be delivered in two qualities with different toughness properties. 1) Quality for low service temperature with minimum impact energy at - 40 °C (N-A-XTRA® M) in a thickness range from 3 to 100 mm. 2) Special quality for low service temperature with minimum impact energy at - 60 °C (classic N-A-XTRA®) in a thickness range from 3 to 50 mm.

Application: The steels are used for welded constructions of all kinds, such as pressure vessels, penstocks, bridges and structures, as well as transport vehicles, mobile cranes, mining equipment, hoistings and earth moving equipment, which are utilized in different types of climatic conditions.

If continuous yielding occurs, the yield strength is determined as Rp0,2

Information Provided by Thyssen Krupp

Key Words: S620QL1; EN 1.8987
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  >= 470 MPa
@Strain 0.2 %,
Temperature 400 °C
>= 68200 psi
@Strain 0.2 %,
Temperature 752 °F
 >= 485 MPa
@Strain 0.2 %,
Temperature 350 °C
>= 70300 psi
@Strain 0.2 %,
Temperature 662 °F
 >= 500 MPa
@Strain 0.2 %,
Temperature 300 °C
>= 72500 psi
@Strain 0.2 %,
Temperature 572 °F
 >= 520 MPa
@Strain 0.2 %,
Temperature 250 °C
>= 75400 psi
@Strain 0.2 %,
Temperature 482 °F
 >= 540 MPa
@Strain 0.2 %,
Temperature 200 °C
>= 78300 psi
@Strain 0.2 %,
Temperature 392 °F
 >= 570 MPa
@Strain 0.2 %,
Temperature 150 °C
>= 82700 psi
@Strain 0.2 %,
Temperature 302 °F
 >= 590 MPa
@Strain 0.2 %,
Temperature 100 °C
>= 85600 psi
@Strain 0.2 %,
Temperature 212 °F
Elongation at Break >= 15 %>= 15 %
Charpy Impact  27.0 J
@Temperature -60.0 °C
19.9 ft-lb
@Temperature -76.0 °F
Transverse
 30.0 J
@Temperature -40.0 °C
22.1 ft-lb
@Temperature -40.0 °F
Transverse
 30.0 J
@Temperature -60.0 °C
22.1 ft-lb
@Temperature -76.0 °F
Longitudinal
 35.0 J
@Temperature -20.0 °C
25.8 ft-lb
@Temperature -4.00 °F
Transverse
 40.0 J
@Temperature -40.0 °C
29.5 ft-lb
@Temperature -40.0 °F
Longitudinal
 40.0 J
@Temperature 0.000 °C
29.5 ft-lb
@Temperature 32.0 °F
Transverse
 50.0 J
@Temperature -20.0 °C
36.9 ft-lb
@Temperature -4.00 °F
Longitudinal
 60.0 J
@Temperature 0.000 °C
44.3 ft-lb
@Temperature 32.0 °F
Longitudinal
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 1.5 %<= 1.5 %
Carbon, C <= 0.20 %<= 0.20 %
Chromium, Cr <= 1.5 %<= 1.5 %
Iron, Fe >= 93.8 %>= 93.8 %As Balance
Manganese, Mn <= 1.6 %<= 1.6 %
Molybdenum, Mo <= 0.60 %<= 0.60 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.80 %<= 0.80 %
Sulfur, S <= 0.010 %<= 0.010 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North American Northern Red Oak Wood
ThyssenKrupp PAS 700 Structural Steel for Cold Forming
ASTM A131 Steel, Grade CS
American White Oak Wood
American Red Oak Wood

NTHYSS019 / 90339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.