MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE FM-2163 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink FM-2163 is a general purpose thermoplastic elastomer available in Nat, Blk, and other colors, used in a variety of automotive applications including interior parts. Sarlink FM-2163 is a medium hardness, high density, UV resistant grade that exhibits excellent haptics, surface appearance, scratch and mar resistance, has low VOC and fogging, and is suitable for extrusion or injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Colorability; Good Processability; Good Scratch Resistance; Good Surface Finish; High Density; Medium Hardness; High Specific Gravity; Low Fogging; Low VOC; UV Resistant; Wear Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 61
@Time 15.0 sec
STAND; ASTM D2240
 63
@Time 15.0 sec
HAND; ASTM D2240
Tensile Strength at Break 830 psi20 mm/min; ASTM D412
Tensile Stress at Strain 210 psi
@Strain 100 %
ASTM D412
 310 psi
@Strain 300 %
ASTM D412
Elongation at Break 750 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Zone 1 380 - 400 °F
Zone 2 390 - 410 °F
Zone 3 400 - 420 °F
Zone 4 400 - 420 °F
Zone 5 410 - 430 °F
Die Temperature 420 - 440 °F
Screw Speed 30 - 100 rpm
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1043 / 237534

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.