MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPE FM-2163 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink FM-2163 is a general purpose thermoplastic elastomer available in Nat, Blk, and other colors, used in a variety of automotive applications including interior parts. Sarlink FM-2163 is a medium hardness, high density, UV resistant grade that exhibits excellent haptics, surface appearance, scratch and mar resistance, has low VOC and fogging, and is suitable for extrusion or injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Colorability; Good Processability; Good Scratch Resistance; Good Surface Finish; High Density; Medium Hardness; High Specific Gravity; Low Fogging; Low VOC; UV Resistant; Wear Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  61
@Time 15.0 sec
61
@Time 0.00417 hour
STAND; ASTM D2240
 63
@Time 15.0 sec
63
@Time 0.00417 hour
HAND; ASTM D2240
Tensile Strength at Break 5.72 MPa830 psi20 mm/min; ASTM D412
Tensile Stress at Strain  1.45 MPa
@Strain 100 %
210 psi
@Strain 100 %
ASTM D412
 2.14 MPa
@Strain 300 %
310 psi
@Strain 300 %
ASTM D412
Elongation at Break 750 %750 %ASTM D412
 
Processing PropertiesMetricEnglishComments
Zone 1 193 - 204 °C380 - 400 °F
Zone 2 199 - 210 °C390 - 410 °F
Zone 3 204 - 216 °C400 - 420 °F
Zone 4 204 - 216 °C400 - 420 °F
Zone 5 210 - 221 °C410 - 430 °F
Die Temperature 216 - 227 °C420 - 440 °F
Screw Speed 30 - 100 rpm30 - 100 rpm
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1043 / 237534

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.