MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Armeen DM18D Neutralizing agent
Categories: Other Engineering Material

Material Notes: INCI name: Dimethyl Stearamine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.774 g/cc
@Temperature 70.0 °C
 0.791 g/cc
@Temperature 60.0 °C
 0.795 g/cc
@Temperature 38.0 °C
Viscosity 42.2 cP
@Temperature 55.0 °C
 46.6 cP
@Temperature 45.0 °C
 52.2 cP
@Temperature 35.0 °C
 63.1 cP
@Temperature 25.0 °C
Vapor Pressure <= 0.000133322 bar
@Temperature 20.0 °C
 0.000660 bar
@Temperature 167 °C
 1.01325 bar
@Temperature 315 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.500 BTU/lb-°F
@Temperature 50.0 °C
 0.540 BTU/lb-°F
@Temperature 25.0 °C
Melting Point 22.0 °C
Boiling Point 160 °C
@Pressure 0.0000666612 MPa
Pour Point 24.0 °C
Flash Point >= 150 °C
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %
 
Descriptive Properties
Amine number180-191 mg KOH/g
AppearanceLiquid
Color= 100 Apha
Content= 1 %Primary + Secondary Amine
 = 95 %Tertiary Amine
 294-312 g/eqNeutralization equivalent
Equivalent mass306 g/eq
HLB71Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY196 / 285719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.