MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Armeen DM18D Neutralizing agent
Categories: Other Engineering Material

Material Notes: INCI name: Dimethyl Stearamine

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.774 g/cc
@Temperature 70.0 °C
0.0280 lb/in³
@Temperature 158 °F
 0.791 g/cc
@Temperature 60.0 °C
0.0286 lb/in³
@Temperature 140 °F
 0.795 g/cc
@Temperature 38.0 °C
0.0287 lb/in³
@Temperature 100 °F
Viscosity  42.2 cP
@Temperature 55.0 °C
42.2 cP
@Temperature 131 °F
 46.6 cP
@Temperature 45.0 °C
46.6 cP
@Temperature 113 °F
 52.2 cP
@Temperature 35.0 °C
52.2 cP
@Temperature 95.0 °F
 63.1 cP
@Temperature 25.0 °C
63.1 cP
@Temperature 77.0 °F
Vapor Pressure  <= 0.000133322 bar
@Temperature 20.0 °C
<= 0.0999998 torr
@Temperature 68.0 °F
 0.000660 bar
@Temperature 167 °C
0.495 torr
@Temperature 333 °F
 1.01325 bar
@Temperature 315 °C
760.000 torr
@Temperature 599 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity  2.09 J/g-°C
@Temperature 50.0 °C
0.500 BTU/lb-°F
@Temperature 122 °F
 2.26 J/g-°C
@Temperature 25.0 °C
0.540 BTU/lb-°F
@Temperature 77.0 °F
Melting Point 22.0 °C71.6 °F
Boiling Point 160 °C
@Pressure 0.0000666612 MPa
320 °F
@Pressure 0.00966587 psi
Pour Point 24.0 °C75.2 °F
Flash Point >= 150 °C>= 302 °F
 
Component Elements PropertiesMetricEnglishComments
H2O, Water <= 0.50 %<= 0.50 %
 
Descriptive Properties
Amine number180-191 mg KOH/g
AppearanceLiquid
Color= 100 Apha
Content= 1 %Primary + Secondary Amine
 = 95 %Tertiary Amine
 294-312 g/eqNeutralization equivalent
Equivalent mass306 g/eq
HLB71Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY196 / 285719

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.