MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Application: wear liners, sliding plates

Information provided by Schwartz Technical Plastics GmbH. Schwartz was acquired by Röchling in 2018.

Key Words: UHMW-PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO R 1183
Moisture Absorption at Equilibrium 0.00 %DIN 53473
Water Absorption at Saturation >= 0.10 %
@Temperature 20.0 °C
ISO R 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 57.0 MPaHc 30; ISO 2039; partially
Tensile Strength, Yield 39.0 MPaISO-DIS 527
Creep Strength 3.20 MPa1% elongation, 1000 h; DIN 53444
 5.00 MPa2% elongation, 1000 h; DIN 53444
Tensile Modulus 1100 MPaDIN 53457
Flexural Strength 40.0 MPaDIN 54352
Flexural Modulus 790 MPaDIN 53457
Compressive Strength 16.0 MPa5% pressing; EN ISO 604
 25.0 MPa10% pressing; EN ISO 604
 32.0 MPa20% pressing; EN ISO 604
Izod Impact, Notched (ISO) NBDIN 53453
Izod Impact Resistance NBswinging hammer 0,1 DIN 51222; DIN 53453
Coefficient of Friction 0.020 - 0.080With lubrication
Coefficient of Friction, Dynamic 0.29no lube; Steel 2162, Rvst=2E-6m, p=0.05 Mpa, v=0.6 m/s, t=40°C
Tear Strength Test 4.5ISO-DIS 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmDIN 53482
Surface Resistance 1.00e+14 ohmDIN 53482
Dielectric Constant 2.3DIN 53483
Dielectric Strength 100 kV/mmDIN 53481
Dielectric Loss Index 0.00010DIN 53483
 
Thermal PropertiesOriginal ValueComments
CTE, linear 200 µm/m-°C
@Temperature 20.0 - 100 °C
DIN 53752
Specific Heat Capacity 2.30 J/g-°C
Thermal Conductivity 0.330 W/m-KDIN 52612
Melting Point 136 °CISO R 1218
Maximum Service Temperature, Air 80.0 °CContinuous
 120 °CIntermittent
Minimum Service Temperature, Air -100 °CContinuous
 
Descriptive Properties
Creepage/leakage ResistanceKA3cDIN 53480
Friction Wear1 micron/km

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wingate Alloys Winco Poly NLT Engineered UHMW
Mitsubishi Chemical Advanced Materials TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet)
Westlake Plastics Lennite® Biocompatible Implant Grade UHMW-PE
Mitsubishi Chemical Advanced Materials TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet)
CENTROPLAST CENTROLEN PE-UHMW Ultra-high molecular weight polyethylene

PSCHW029 / 90226

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.