MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials TIVAR® Polysteel Filled UHMW-PE, High Specific Gravity (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6464ASTM D2240
Tensile Strength 19.3 MPa2800 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 125 %125 %ASTM D638
Tensile Modulus 0.421 GPa61.0 ksiASTM D638
Flexural Modulus 0.752 GPa109 ksiASTM D790
Compressive Strength 24.8 MPa3600 psi10% Def.; ASTM D695
Compressive Modulus 0.579 GPa84.0 ksiASTM D695
Coefficient of Friction, Dynamic 0.140.14Dry vs. Steel; QTM55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+10 ohm>= 1.00e+10 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 127 °C260 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters LimitedLimited
 
Descriptive Properties
Machinability31-10, 1=Easier to Machine

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wingate Alloys Winco Poly NLT Engineered UHMW
Mitsubishi Chemical Advanced Materials TIVAR™ CERAM P UHMW-PE, Premium Microsphere Filled
Mitsubishi Chemical Advanced Materials TIVAR™ HPV FG UHMW-PE
Mitsubishi Chemical Advanced Materials QuickSilver™ UHMW-PE Premium Truck Lining
Röchling LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene

P1SMP19 / 20169

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.