MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Cerox® 90V Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Metal Melting Crucibles. Cerox fired refractory shapes are thixotropically cast using a dispersion agent, which allows the Cerox mix to flow when vibrated without requiring a high water content. These manufacturing techniques, combined with precisely controlled firing and 100% product inspection, produce high-quality omponents suited to the most arduous of high-temperature environments. Cerox refractory shapes are dense, hard, and chemically stable, offering resistance to acids, slags, and gases.

Applications:

  • Combustion chambers and components
  • Burner blocks
  • Pipes
  • Gas reactor components
  • Wear plates
  • Crucibles
  • Nozzles
  • Resistance heater hangers, holders, etc.
  • Runners
  • Induction blocks
  • Tundish boxes
  • Distribution plates
  • Skid rails
  • Rabble blocks and teeth
  • Saggers
  • Setters
  • Pusher tiles
  • Tubes
  • Plates
  • Muffles
  • Piers

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.885 g/cc
Porosity 20 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0172 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.10 µin/in-°F
 
Component Elements PropertiesOriginal ValueComments
Al2O3 91 %
CaO+MgO 0.040 %
Fe2O3 0.15 %
K2O+Na2O 0.15 %
SiO2 8.0 %
TiO2 0.10 %
 
Descriptive Properties
Classification Temperature (°C)1699

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Morgan Advanced Ceramics AL 1009™ Mac-A100W-Porous Aluminum Oxide Ceramic
Morgan Advanced Ceramics BTU-Block ™ Flexible Thermal Ceramic
Morgan Advanced Ceramics IFB Insulation Range JM™ 23-400 Thermal Ceramic
Morgan Advanced Ceramics Cerachrome® Refractory Ceramic Fiber Bulks Thermal Ceramic

CMORF6075 / 202859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.