MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: RCF Fiber Class. Kaowool Millboard products are processed from a slurry consisting of Kaowool ceramic fibers, fillers and binders. The fiber raw material is kaolin, a naturally occurring high-purity alumina-silica fireclay. Kaowool Millboard products are strong, thin, durable ceramic fiber based boards having a variety of high-temperature applications. Although these products were formulated and designed to replace asbestos millboard, their potential use extends into more conventional refractory fiber applications. Their use should be considered whenever there is a need for a thin, durable board with excellent insulating characteristics. Kaowool 822 Millboard is a high density, strong board with many applications including fire protection, thermal barriers and backup insulation.

Applications:

  • High-temperature gaskets (all grades) High-temperature roll covering (grade 822)
  • Fire protection (grade 822)
  • Thermal barrier (grades 822 and 1401)
  • Backup insulation (grades 822 and 1401)

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.881 g/cc0.0318 lb/in³
Loss On Ignition 5.0 - 7.0 %5.0 - 7.0 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.340 - 0.510 MPa49.3 - 74.0 psiat 5% deformation
 0.690 - 0.860 MPa100 - 125 psiat 10% deformation
 1.72 - 2.06 MPa249 - 299 psiat 15% deformation
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.110 W/m-K
@Temperature 260 °C
0.763 BTU-in/hr-ft²-°F
@Temperature 500 °F
ASTM C201
 0.130 W/m-K
@Temperature 538 °C
0.902 BTU-in/hr-ft²-°F
@Temperature 1000 °F
ASTM C201
 0.140 W/m-K
@Temperature 816 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 1500 °F
ASTM C201
 0.160 W/m-K
@Temperature 1093 °C
1.11 BTU-in/hr-ft²-°F
@Temperature 1999 °F
ASTM C201
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air <= 1093 °C<= 1999 °FContinuous Use
 
Component Elements PropertiesMetricEnglishComments
Al2O3 35 %35 %
Other 2.0 %2.0 %
SiO2 63 %63 %
 
Descriptive Properties
Classification Temperature (°C)1260
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics IFB Insulation Range JM™ 23-400 Thermal Ceramic
Morgan Advanced Ceramics BTU-Block ™ Panel Thermal Ceramic

CMORF6068 / 202852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.