MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2080415D2 Silver Counter Electrode Paste
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: This product is a screen printable polymer paste designed as a counter electrode in electrochemical biosensors. This ink can be used in conjunction with our working carbon electrode ink C2030519P4, to increase the conductivity of the carbon by printing tracks underneath.
Low silver content
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156-325tpi
Substrate: Polyimide, PET, PEN

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 44 - 46 %
@Temperature 700 °C
Viscosity 900 - 1100 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 10.0 - 25.0 microns
Storage Temperature 20.0 °Csealed container
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.015 - 0.020 ohm
@Thickness 0.0250 mm
Printed onto 125 µm PET film
 0.030 - 0.045 ohm
@Thickness 0.0100 mm
Printed onto 125 µm PET film
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 minbelt dryer
 10.0 min
@Temperature 150 °C
 15.0 min
@Temperature 135 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Conductive Filler TypeSilver (Ag)
Coverage cm2/g250-270Using a 230 mesh stainless steel screen
Material TypeReady-To-Use Formulation
Recommended SubstratesPolyimide, PET, PEN
Solvent SystemEthoxy Propanol or Sericol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Indalloy 215 Silver Solder Alloy
Nickel silver 65-10, UNS C74500, OSO70 Temper flat products
Oxygen-free silver-bearing Copper, UNS C10400, H00 Temper flat products
Potters Industries Conduct-O-Fil® AG-SL150-16-TRD Silver-coated Hollow Ceramic Spheres
Silver Aluminum Selenide, AgAlSe2

WGELZ9018 / 139331

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.