MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free silver-bearing Copper, UNS C10400, H00 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: auto gaskets, radiators, busbars, conductivity wire, contacts, radio parts, winding, switches, terminals, commutator segments, chemical process equipment, printing rolls, clad metals, printed circuit foil.

Test specimens: flat products - 1mm and 6mm thicknesses.

Similar alloys distinguished only by silver content: 8 oz/ton Ag (UNS C10400), 10 oz/ton Ag (UNS C10500), 25 oz/ton Ag (UNS C10700).

Key Words: AMSIL Copper; Oxygen-free Silver-Copper; ASTM-B-152, QQ-C-502, QQ-C-576
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³UNS C10700
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 1010
Hardness, Rockwell F 6060
Hardness, Rockwell 30T 25
@Thickness 1.00 mm
25
@Thickness 0.0394 in
Flat products
Tensile Strength, Ultimate 250 MPa36300 psi
Tensile Strength, Yield 195 MPa28300 psi
Elongation at Break  30 %
@Thickness 1.00 mm
30 %
@Thickness 0.0394 in
In 50 mm
 40 %
@Thickness 6.00 mm
40 %
@Thickness 0.236 in
In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 170 MPa24700 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000172 ohm-cm
@Temperature 20.0 °C
0.00000172 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C0.0920 BTU/lb-°F
Thermal Conductivity 388 W/m-K
@Temperature 20.0 °C
2690 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point <= 1083 °C<= 1981 °F
Solidus 1083 °C1981 °F
Liquidus 1083 °C1981 °F
Annealing Point >= 482 °C>= 900 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 475 - 750 °C887 - 1380 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.95 %>= 99.95 %Includes Ag
Silver, Ag >= 0.027 %>= 0.027 %Min 8 troy oz./ton

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free silver-bearing Copper, UNS C10400, OSO25 Temper flat products, tubing
Oxygen-free Copper (OF), UNS C10200, H00 Temper, flat products
Silver Aluminum Sulfide, AgAlS2
Molybdenum Disilicide, MoSi2
Nickel silver 65-10, UNS C74500, OSO70 Temper flat products

MC10400b3 / 10419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.