MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol TR 016 Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: A blend of fatty acid metal soap and an amide

The amide of STRUKTOL® TR 016 has sites available for hydrogen bonding, and is therefore able to act as a physical coupling agent between polymer systems and a range of filler materials. This permits STRUKTOL® TR 016 to act as an efficient blending or dispersing agent in highly filled systems, providing a more uniform and homogenous initial mix. At processing conditions, STRUKTOL® TR 016 is an effective internal lubricant for the polyolefins, PVC, PS, ABS and many of the TPO systems. Application areas recommended for STRUKTOL® TR 016 in highly-filled systems include TPEs and TPO compounds, filled olefins, flame retarded polymers and color concentrate materials. In addition, STRUKTOL® TR 016 can be useful in those standard unfilled polymers where reduced viscosity and improved flow are desirable at processing conditions. In many systems, better surface appearance and lower and more uniform mold shrinkage will be seen. Physical property losses are quite small for most compounds at normal addition levels of STRUKTOL® TR 016. Benefits of STRUKTOL® TR 016 include:

  • Improved flow at processing temperatures
  • Better surface appearance
  • Easier mold release in many systems
  • Better dispersion of fillers and additives
  • Non-blooming properties

FDA Status: 173.340; 175.105; 175.300; 175.320; 176.170; 176.200; 176.210; 177.1200; 177.2260; 177.2410; 177.2600; 177.2010; 178.2010; 178.3860; 181.29; 184.1229

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Additive Loading 0.25 - 1.0 %
 
Thermal PropertiesOriginal ValueComments
Dropping Point 96.0 - 108 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 24.0 Month
 
Descriptive Properties
AppearancePale beads or pastilles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silon Taboradd 23-08350 Processing Aid Masterbatch
Shandong Rike Chemical HELI™ HL-220N PVC Processing Aid Series (PA)
LG Chemical PA828 Processing aid
Ineos R08S-00 Polypropylene Random Copolymer
Struktol TR 060 Blending Aid, Processing Additive

PSTRUK00 / 69228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.