MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
NextGen Adhesives TC907-33 Thermally Conductive Adhesive
Categories: Polymer; Adhesive

Material Notes: Description: NGAC TC907-33 is a thermally conductive and electrically insulating adhesive which can be cured at room temperature. It was designed for assembling heat sensitive components onto printed circuit boards. It is recommended for any application requiring strong adhesive bonds and excellent thermal transfer.

Advantages and Applications: NGAC TC907-33 provides strong and high impact bonds which improve heat transfer while maintaining electrical insulation. It bonds to a wide range of substrates including metals, glass and plastics. The NGAC TC907-33 has a low coefficient of thermal expansion and will provide excellent resistance to mismatched substrates and very low shrinkage. Additionally, the NGAC TC907-33 is highly resistant to chemicals.

Information Provided by Nextgen Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.98 g/cc
Viscosity 115000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Shear Strength 3000 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
Thermal Conductivity 2.39 W/m-K
Maximum Service Temperature, Air 125 °C
Minimum Service Temperature, Air -70.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 120 - 240 min
@Temperature 65.0 °C
 1440 min
@Temperature 25.0 °C
Pot Life 40 min
 
Descriptive Properties
ColorBlue
Mix Ratio by Weight (R/H)100/9.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow TC-5688 Thermally Conductive Compound
Dow TC-5022 Thermally Conductive Compound
Cotronics Resbond™ 920 High Temperature Ceramic Adhesive, Thermally Conductive
Cotronics 454B Machinable Non-Sag Putty Adhesive
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive

PNEXT011 / 90258

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.