MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Cotronics 454B Machinable Non-Sag Putty Adhesive
Categories: Polymer; Thermoset; Epoxy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.90 g/cc0.0686 lb/in³
Moisture Absorption at Equilibrium 0.20 %0.20 %
Viscosity 100000 cP100000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Ultimate 68.9 MPa10000 psi
Elongation at Break 1.2 %1.2 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cm
Dielectric Strength 17.7 kV/mm450 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
44.4 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 5.04 W/m-K35.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 232 °C450 °F
Shrinkage 0.20 %0.20 %
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min
@Temperature 121 °C
0.500 hour
@Temperature 250 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ MT-220 Thermally Conductive Adhesive
Lord Adhesives Thermoset™ MT-125 Thermally Conductive Adhesive
Lord Adhesives Thermoset™ MD-200 Electrically Conductive Die-Attach Adhesive
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy
Dow TC-5688 Thermally Conductive Compound

PCOTR0450 / 29070

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.