MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives Thermoset™ MT-220 Thermally Conductive Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Thermoset™ MT-220 thermally conductive adhesive is a fast cure, one-component adhesive designed for use as a thermal interface adhesive for heat sink attachment and other applications requiring superior adhesion strength and extremely high thermal conductivity.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.49 g/cc2.49 g/cc
Brookfield Viscosity  45000 cP
@Temperature 25.0 °C
45000 cP
@Temperature 77.0 °F
Spindle 6 @ 10rpm
 100000 cP
@Temperature 25.0 °C
100000 cP
@Temperature 77.0 °F
Spindle 6 @ 1rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272
Modulus of Elasticity 0.156 GPa22.6 ksiStorage
Shear Strength 6.21 MPa
@Temperature 900.45 °C
900 psi
@Temperature 1652.8 °F
Lap
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.0 µm/m-°C13.9 µin/in-°FAlpha 1
 82.0 µm/m-°C45.6 µin/in-°FAlpha 2
Thermal Conductivity 4.20 W/m-K29.1 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg -90.0 °C-130 °FTMA
 
Processing PropertiesMetricEnglishComments
Cure Time  10.0 min
@Temperature 150 °C
0.167 hour
@Temperature 302 °F
 30.0 min
@Temperature 125 °C
0.500 hour
@Temperature 257 °F
Pot Life 10080 min
@Temperature 25.0 °C
10080 min
@Temperature 77.0 °F
Shelf Life 6.00 Month
@Temperature -40.0 °C
6.00 Month
@Temperature -40.0 °F
 
Descriptive Properties
AppearanceGray
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ MT-125 Thermally Conductive Adhesive
Lord Adhesives Thermoset™ MD-200 Electrically Conductive Die-Attach Adhesive
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy
Dow TC-5688 Thermally Conductive Compound
Dow TC-5022 Thermally Conductive Compound

PLORD035 / 86043

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.