Pyrotek TS-180 Thermoset Electrical Insulation Product
Categories:
Polymer
;
Thermoset
;
Epoxy
;
Filled/Reinforced Thermoset
Material Notes:
Glass reinforcement, Epoxy Resin, Straw Color. Excellent mechanical and electrical properties at elevated temperature.
Information provided by Pyrotek.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.842
g/cc
0.06655
lb/in³
Water Absorption
0.20 %
0.20 %
Mechanical Properties
Metric
English
Comments
Flexural Strength
350
MPa
50800
psi
Compressive Strength
400
MPa
58000
psi
Electrical Properties
Metric
English
Comments
Dielectric Strength
10.0
kV/mm
254
kV/in
Thermal Properties
Metric
English
Comments
Maximum Service Temperature, Air
160
°C
320
°F
Continuous
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Tra-Con Tra-Bond 216R02 Quick Set Electrical Insulator
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade
PPYRO050 / 58383
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.