MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond 216R02 Quick Set Electrical Insulator
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 216R02 is an exceptional epoxy formulation recommended for applications where both quick set-up and a low-viscosity material are required. This clear, two-part, low-viscosity system is easily mixed at room temperature, contains no solvents, and is suitable for high-performance structural applications. It develops tough, strong bonds to plastics, glass, ceramics, rubber, metals, and various other substrates. Fully cured TRA-BOND 216R02 is an excellent electrical insulator.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccMixed
Viscosity 2000 cP2000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 25.0 °C77.0 °FUltimate Tg; DSC
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hour1 hr @ 25°C + 2 hrs @ 65°C
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Pot Life 5.00 min
@Temperature 25.0 °C
5.00 min
@Temperature 77.0 °F
 
Descriptive Properties
Color ClearMixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy
Pyrotek TS-180 Thermoset Electrical Insulation Product
Cosmic Plastics E484 Glass Filled Epoxy Molding Compound, Electrical Grade

PTRAC054 / 70982

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.