MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hybrid Plastics FireQuench® PM 1287 Resin
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset

Material Notes: FireQuench® PM1287 is an optically transparent, fire retardant hybrid nanocomposite resin that can serve as a replacement for standard epoxy-vinyl ester and related resins. It can be employed as an unfilled, nanocomposite resin or it can be filled and utilized with reinforcements such as glass fiber. FireQuench® PM1287 has significantly improved thermal and flame retardant properties when compared to all other high temperature thermoset resins.

Information provided by Hybrid Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Viscosity 100 cP
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 1.7 %composite
 3.5 %resin
Flexural Strength 13513 psi
@Temperature 23.0 °C
resin
 67200 psi
@Temperature 23.0 °C
composite
Flexural Modulus 140000 psi
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature <= 600 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Gel Time 45.0 - 60.0 min
@Temperature 60.0 °C
with 0.2%wt catalyst load
Shelf Life 24.0 - 36.0 Monthw/o catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Hexcel® HexForce™ 383 Aramid Fabric
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
Overview of materials for Polypropylene Copolymer
Hexcel® HexForce™ 328 Aramid Fabric

PHYBR019 / 78829

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.