MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses strong dimensional stability and chemical resistance. In addition, the effect of water absorption, which is a traditional weakness of polyamides, has been reduced to a minimum.

Applications:

  • Cylinder head covers
  • Thermostat cases
  • Oil pump housings
  • Hydraulic system pistons
  • Cooling system parts
  • Roller/pulley parts

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ASTM D792
Filler Content 15 %15 %
Water Absorption  0.4 %
@Thickness 2.00 mm
0.4 %
@Thickness 0.0787 in
24 hours in 23°C water; ASTM D570
 2.5 %
@Thickness 2.00 mm
2.5 %
@Thickness 0.0787 in
24 hours in 100°C water; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 2.00 mm
0.0060 in/in
@Thickness 0.0787 in
Vertical Direction; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiASTM D638
Elongation at Break 3.0 %3.0 %Measured between the chucks; ASTM D638
Flexural Strength 170 MPa24700 psiASTM D790
Flexural Modulus 5.50 GPa798 ksiASTM D790
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.0 µm/m-°C
@Temperature 20.0 °C
30.6 µin/in-°F
@Temperature 68.0 °F
Vertical Direction; ASTM D696
CTE, linear, Parallel to Flow 34.0 µm/m-°C
@Temperature 20.0 °C
18.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Melting Point 320 °C608 °F
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FASTM D648
Glass Transition Temp, Tg 125 °C257 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Feed Temperature 50.0 - 90.0 °C122 - 194 °FHopper Bottom Temp for Mechanical and Structural Standard Molding
 50.0 - 90.0 °C122 - 194 °FHopper Bottom for Electronic and Electric Standard Molding
Nozzle Temperature 315 - 335 °C599 - 635 °FNH Cylinder Temp for Electronic and Electric Standard Molding
 325 - 340 °C617 - 644 °FNH Cylinder Temp for Mechanical and Structural Standard Molding
Zone 1 300 - 325 °C572 - 617 °FC1 Cylinder Temp for Electronic and Electric Standard Molding
 315 - 330 °C599 - 626 °FC1 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 2 315 - 335 °C599 - 635 °FC2 Cylinder Temp for Electronic and Electric Standard Molding
 320 - 335 °C608 - 635 °FC2 Cylinder Temp for Mechanical and Structural Standard Molding
Zone 3 320 - 335 °C608 - 635 °FC3 Cylinder Temp for Electronic and Electric Standard Molding
 325 - 340 °C617 - 644 °FC3 Cylinder Temp for Mechanical and Structural Standard Molding
Mold Temperature 90.0 - 140 °C194 - 284 °Ffor Mechanical and Structural Standard Molding
 90.0 - 140 °C194 - 284 °Ffor Electronic and Electric Standard Molding
Screw Speed 150 rpm150 rpmfor Mechanical and Structural Standard Molding
 150 rpm150 rpmfor Electronic and Electric Standard Molding
 
Descriptive Properties
Injection PressureMediumElectronic and Electric Standard Molding
 MediumMechanical and Structural Standard Molding
Injection SpeedMediumElectronic and Electric Standard Molding
 MediumMechanical and Structural Standard Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui Arlen™ PA MXD6 40% Glass Fiber-Reinforced Modified Nylon 6T (COND)
Mitsui Arlen™ PPS 40% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM)
Mitsui Arlen™ AE2230 30% Glass Fiber-Reinforced Modified Nylon 6T, for Tribolic Applications (COND)
Mitsui Arlen™ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (DAM)
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND)

PMIT019 / 53195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.