MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PEARLCOAT® 162K is used in melt coatings on textile substrates, for end-uses in industrial coatings (for life-jackets, etc.) obtained by extrusion and calendaring. PEARLCOAT® 162K is used for obtaining extruded films and fabric coatings.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282ASTM D2240
Tensile Strength, Yield 30.05 MPa4359 psiASTM D412
Elongation at Break 550 %550 %ASTM D412
50% Modulus 4.00 MPa
@Strain 50 %
4.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 5.01 MPa
@Strain 100 %
727 psi
@Strain 100 %
ASTM D412
300% Modulus 10.02 MPa
@Strain 300 %
1453 psi
@Strain 300 %
ASTM D412
Tear Strength 68.0 kN/m388 pliUnnicked; ISO 34-1B
Abrasion 2525Resistance (mm³); ISO 4649-A
 
Processing PropertiesMetricEnglishComments
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour
Dew Point <= -30.0 °C<= -22.0 °F
 
Descriptive Properties
Roll 1160°C
Roll 2170°C
Rubber Roll 3not heated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Austin Novel Materials Texalan® 598A Polyether-based TPU
Austin Novel Materials Texalan® 698A Polyester and Polyether based TPU
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude

PMES66 / 88443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.