MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® ETE 75DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).

Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency and UV stability.

Uses: Extrusion: Hose and Tube, Profile, Cable Jacket. Injection molding: Various.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 72 - 78
@Time 5.00 sec
72 - 78
@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 40.7 MPa5900 psiASTM D412
Elongation at Break 330 %330 %ASTM D412
100% Modulus 22.0 MPa
@Strain 100 %
3190 psi
@Strain 100 %
ASTM D412
300% Modulus 27.0 MPa
@Strain 300 %
3920 psi
@Strain 300 %
ASTM D412
Tear Strength 26.3 kN/m150 pliTrouser; ASTM D470
Graves Tear Strength 245 kN/m1400 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 68
@Load 1.00 kg
68
@Load 2.20 lb
H-18 wheel; ASTM D3389
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °FDSC
Glass Transition Temp, Tg -10.0 °C14.0 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 204 °C399 °FExtrusion
Zone 2 210 °C410 °FExtrusion
Zone 3 216 °C421 °FExtrusion
Zone 4 216 °C421 °FExtrusion
Adapter Temperature 216 °C421 °F5, Extrusion
Die Temperature 218 °C424 °F6, Zone 1, Extrusion
 218 °C424 °FZone 2, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU

PNOVEON591 / 121482

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.