MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach UgiPerm™ 12FM Stainless Steel Bar
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Description: UgiPerm™ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was developed for magnetic applications requiring a very low coercive magnetic field (Hc) and a very high permeability. UgiPerm™ 12FM has a high level of electrical resistivity that shortens activation time when used in pulse mode. It offers excellent magnetic properties with superior corrosion resistance no offered by iron alloys.

Applications: Solenoid valves, fuel injectors, irrigation valves, magnetic sensors, magnetic brakes, and electro-mechanical devices.

Magnetic Properties (Heat Treatment): Uniformly heat at 800°/900°C (1470°F/1650°F) for 2 hours, then cool to 500°C (930°F) at a rate of 50°C (120°F) per hour. The cycle should be done in a dry hydrogen or vacuum atmosphere to prevent oxidation.

Information provided by Schmolz + Bickenbach

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.279 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 87 - 92
Tensile Strength 65.0 - 80.0 ksi
@Thickness <=25.4 mm
Cold Drawn Bar
Tensile Strength, Yield 45.0 - 65.0 ksi
@Strain 0.2 %,
Thickness <=25.4 mm
Cold Drawn Bar
Elongation at Yield >= 30 %
@Thickness <=25.4 mm
Cold Drawn Bar
Reduction of Area >= 60 %
@Thickness <=25.4 mm
Cold Drawn Bar
Tensile Modulus 29000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000780 ohm-cm
Magnetic Permeability 2000 - 3000
Magnetic Coercive Force, Hc 1.2 - 1.6 Oe
Magnetic Saturation Flux Density, Bmax 17000 Gauss
Magnetic Remanence, Br 5000 - 7000 Gauss
Curie Temperature 1350 °F
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.75 µin/in-°F
@Temperature 20.0 - 100 °C
 6.00 µin/in-°F
@Temperature 20.0 - 204 °C
 6.40 µin/in-°F
@Temperature 20.0 - 299 °C
 6.50 µin/in-°F
@Temperature 20.0 - 432 °C
 6.80 µin/in-°F
@Temperature 20.0 - 499 °C
Thermal Conductivity 152 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1290 - 1470 °F
@Time 3600 sec
Soft; Air cool
Hot-Working Temperature 900 °FFlow Stress of 110 MP at 3.6s-1
 1000 °FFlow Stress of 65 MP at 3.6s-1
 1100 °FFlow Stress of 40 MP at 3.6s-1
 1200 °FFlow Stress of 25 MP at 3.6s-1
 1380 - 2190 °FUniformly heating
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %
Chromium, Cr 11.5 - 12.5 %
Iron, Fe >= 83.44 %
Manganese, Mn 0.30 - 0.50 %
Molybdenum, Mo 0.25 - 0.75 %
Nickel, Ni >= 0.50 %
Phosphorus, P <= 0.040 %
Silicon, Si 1.0 - 2.0 %
Sulfur, S 0.15 - 0.25 %
 
Descriptive Properties
Corrosion ResistanceHumidity3/4
 NaCl 0.2g/l1.65% mass loss; 60°C; 500 hrs
 NaCl 0.4g/l1.6% mass loss; 60°C; 500 hrs
 NaCl 0.6g/l2.4% mass loss; 60°C; 500 hrs
 Nitric Acid2/4
 Sodium Carbonate2/4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach 430FR Stainless Steel Bar
FloMet 430L Stainless Steel
Sandvik 2002 Precision Wire
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel

NSCHMO042 / 125915

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.