MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® F593 Epoxy Resin, W3G282 Carbon Fabric
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Hexcel designation: W3G282-42"-F593; Fiber: Amoco T-300/3k

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2.965 MPa
@Temperature 93.0 °C
Sandwich Flatwise Tension, Wet
 3.896 MPa
@Temperature 93.0 °C
Sandwich Flatwise Tension, Dry
 4.682 MPa
@Temperature -59.0 °C
Sandwich Flatwise Tension, Dry
 4.806 MPa
@Temperature 24.0 °C
Sandwich Flatwise Tension, Dry
 419 MPa
@Temperature 71.0 °C
Wet
 420 MPa
@Temperature 93.0 °C
Dry
 462 MPa
@Temperature 71.0 °C
Dry
 485 MPa
@Temperature -54.0 °C
Dry
 637 MPa
@Temperature 24.0 °C
Dry
Tensile Modulus 49.6 GPa
@Temperature 71.0 °C
Wet
 51.7 GPa
@Temperature 71.0 °C
Dry
 53.8 GPa
@Temperature 93.0 °C
Dry
 55.2 GPa
@Temperature -54.0 °C
Dry
 56.5 GPa
@Temperature 24.0 °C
Dry
Compressive Yield Strength 410 MPa
@Temperature 71.0 °C
Wet
 469 MPa
@Temperature 93.0 °C
Dry
 536 MPa
@Temperature 71.0 °C
Dry
 627 MPa
@Temperature 24.0 °C
Dry
 745 MPa
@Temperature -59.0 °C
Dry
Compressive Modulus 44.8 GPa
@Temperature 71.0 °C
Wet
 46.9 GPa
@Temperature 93.0 °C
Dry
 48.3 GPa
@Temperature 71.0 °C
Dry
 50.3 GPa
@Temperature -59.0 °C
Dry
 51.0 GPa
@Temperature 24.0 °C
Dry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F593 Epoxy Resin, W3T282 Carbon Fabric
Hexcel® HexPly® F522 Epoxy Resin, F3C433 Carbon Fabric
Hexcel® HexPly® F522 Epoxy Resin, F3C584 Carbon Fabric
Hexcel® HexPly® F593 Epoxy Resin, F3T584 Carbon Fabric
Hexcel® HexPly® F593 Epoxy Resin

PHEXC148 / 98618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.