Notes: Monprene SP-19985 XRD2 is a high performance thermoplastic elastomer designed for a variety of consumer sporting good application including playground flooring requiring a soft, rubber-like feel. Monprene SP-19985 XRD2, available in NAT and colors, is a higher hardness, medium density, UV stabilized grade that exhibit excellent abrasion resistance and is suitable for injection molding. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Abrasion Resistant; Brominated; Filled; Flame Retardant; Good Colorability; High Flow; Medium Density; High Hardness; Light Stabilized; Lubricated; High Flow; Slip; Sunlight Resistant; UV Resistant Uses: Flooring; Rubber Replacement RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding Preliminary data. Information provided by Teknor Apex |