MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Monprene® SP-19985 XRD2 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene SP-19985 XRD2 is a high performance thermoplastic elastomer designed for a variety of consumer sporting good application including playground flooring requiring a soft, rubber-like feel. Monprene SP-19985 XRD2, available in NAT and colors, is a higher hardness, medium density, UV stabilized grade that exhibit excellent abrasion resistance and is suitable for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Abrasion Resistant; Brominated; Filled; Flame Retardant; Good Colorability; High Flow; Medium Density; High Hardness; Light Stabilized; Lubricated; High Flow; Slip; Sunlight Resistant; UV Resistant

Uses: Flooring; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ASTM D792
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
24 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  85
@Time 5.00 sec
85
@Time 0.00139 hour
Injection Molded; ASTM D2240
 87
@Time 1.00 sec
87
@Time 0.000278 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 9.10 MPa1320 psiDie C, 20 in/min, Across Flow; ASTM D412
 9.93 MPa1440 psiDie C, 20 in/min, Flow; ASTM D412
Tensile Stress at Strain  4.87 MPa
@Strain 100 %
706 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 5.77 MPa
@Strain 100 %
837 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 6.32 MPa
@Strain 300 %
917 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 7.45 MPa
@Strain 300 %
1080 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 500 %500 %Die C, 20 in/min, Flow; ASTM D412
 600 %600 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 37.3 kN/m213 pliDie C, 20 in/min, Across Flow; ASTM D624
 44.9 kN/m256 pliDie C, 20 in/min, Flow; ASTM D624
Compression Set  40 %
@Temperature 22.8 °C,
Time 79200 sec
40 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 71 %
@Temperature 70.0 °C,
Time 79200 sec
71 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 20 %20 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 - 216 °C380 - 420 °F
Middle Barrel Temperature 193 - 216 °C380 - 420 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 193 - 216 °C380 - 420 °F
Melt Temperature 193 - 216 °C380 - 420 °F
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.345 MPa25.0 - 50.0 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlue
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0964 / 237455

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.