MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® LJP Polyester Film, 500 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® LJP is an industrial grade very clear film that is available with adhesion promoting coatings and slip coatings. For higher quality end-uses (especially for surface requirements) consider using alternatives such as Melinex® 453, 454 or Mylar® LJ.

General Product Info: The following product Mylar® LJP variants are available: LJP111 One side pretreated to promote adhesion to most printing inks and industrial coatings. LJP112 Two side pretreated to promote adhesion to most printing inks and industrial coatings. LJP181 One side pretreated for slip to provide good handling properties. LJP182 Two side pretreated for slip to provide good handling properties

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³Typical Mylar®; ASTM D1505
Thickness 127 microns5.00 mil
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 96.5 MPa14000 psiASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa14000 psiASTM D882A
Film Elongation at Break, MD 160 %160 %ASTM D882A
Film Elongation at Break, TD 120 %120 %ASTM D882A
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882A
Film Tensile Strength at Break, TD 207 MPa30000 psiASTM D882A
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FTypical Mylar®
Melting Point 254 °C489 °FTypical Mylar® via DSC
Shrinkage, MD 1.0 %
@Temperature 150 °C,
Time 1800 sec
1.0 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.50 %
@Temperature 150 °C,
Time 1800 sec
0.50 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
Haze 1.0 %1.0 %ASTM D1003
Transmission, Visible 87 %87 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® DS Polyester Film
DuPont Teijin Films Mylar® 840 Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 800C Polyester Packaging Film, 48 Gauge
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge

PDTZ9346 / 139666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.