Description: Electrically Conductive - Thermabond®. Bonds with primer. Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Recommended Primers: Dow Coring S2260 Product Use: Electrically conductive electronic adhesive. Bonds with primer. Appearance: Naturally (gray) colored, high viscosity gum (tan or brown after cure) This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications. Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation. |