MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Description: Electrically Conductive - Thermabond®. Bonds with primer.

Design/Construction:
Liner: FEP
Product: Uncured Silicone Rubber
Carrier: PTFE Coated Fiberglass

Recommended Primers: Dow Coring S2260

Product Use: Electrically conductive electronic adhesive. Bonds with primer.

Appearance: Naturally (gray) colored, high viscosity gum (tan or brown after cure)

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.70 g/cc0.134 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns1.00 milLiner
 76.2 microns3.00 milCarrier
 102 microns4.00 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070Silicone Property; ASTM D2240
Tensile Strength 2.65 MPa385 psiSilicone Property; ASTM D412
Elongation at Break 225 %225 %Silicone Property; ASTM D412
Modulus of Elasticity 0.00550 GPa0.798 ksiSilicone Property; Arlon-SAQ-TMS-008
Poissons Ratio 0.500.50Approximately, Silicone Property
Shear Strength 2.76 MPa400 psiLap Shear Strength; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.050 ohm-cm0.050 ohm-cmSilicone Property; ASTM D991
 
Thermal PropertiesMetricEnglishComments
CTE, linear 93.0 µm/m-°C51.7 µin/in-°FASTM E 831
Specific Heat Capacity 0.400 J/g-°C0.0956 BTU/lb-°FSilicone Property; E1461-01
Thermal Conductivity 2.50 W/m-K17.4 BTU-in/hr-ft²-°FSilicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg -116 °C-177 °FSilicone Property; ASTM E 1356
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 141 °C
0.250 hour
@Temperature 285 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 4.44 - 10.0 °C
6.00 Month
@Temperature 40.0 - 50.0 °F
From date of manufacture
 
Descriptive Properties
ColorNaturally Gray
Total Product Weight (g/m2)376Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Rogers Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

PARL490 / 125676

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.