NY-FLEX® E-TPE grades deliver excellent flexibility at low temperature, superior retention of properties to elevated temperature, exceptional impact toughness and resilience. These also exhibit high creep resistance, strong resistance to flex fatigue, good abrasion resistance, and good resistance to greases, oils, and solvents. These materials are block copolymers of nylon (polyamide) segments and polyether segments. Physical properties vary with the ratio of the two components. 'Dry' samples tested as-molded - <0.3% moisture. 'Conditioned' samples are equilibrated at 50% RH and 23°C. Information provided by Nylon Corporation of America. |