MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber
Categories: Ceramic; Oxide

Material Notes: Ceraform 250 Formula based on Cerafiber used for premouled launder linings (aluminium foundries) and 1000 x 1000mm boards. Ceraform is a vacuum-formed insulating product, made from ceramic fibre (Cerafiber, Cerachem, or Cherachrom, fibres as appropriate), refractory constituents and a small percentage of organic binder. The versatility of the vacuum-forming process facilitates the manufacture not only of simple forms, such as tubes, cones and flat panels, but also of geometrically complex shapes, such as burner blocks, fire bases and kiln-car blocks. Also, the basic process is being continually developed to produce new grades to match new and changing customer requirements. Good cohesive strength, high operating temperature and excellent insulating properties make Ceraform ideally suited to a wide and continually expanding range of industrial applications.

Applications:

  • Riser sleeves for ferrous and non-ferrous molten metals
  • Tap-hole cones and launder linings for non-ferrous molten metal’s
  • Doors and combustion chamber linings for boilers
  • Burner blocks
  • Furnace sight holes
  • Kiln car blocks
  • Ferrules for chimney
  • Heating element supports
  • Duct and flue linings
  • Insulation for domestic appliances
  • Pipes insulation
  • Fire protection

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.450 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00300 GPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.100 W/m-K
@Temperature 200 °C
ENV-1094-1
 0.110 W/m-K
@Temperature 400 °C
ENV-1094-1
 0.130 W/m-K
@Temperature 600 °C
ENV-1094-1
 0.170 W/m-K
@Temperature 800 °C
ENV-1094-1
 0.240 W/m-K
@Temperature 1000 °C
ENV-1094-1
Maximum Service Temperature, Air 1260 °CContinuous Use
Shrinkage 3.5 %
 
Component Elements PropertiesOriginal ValueComments
Al2O3 31.3 %
Fe2O3 0.40 %
Loss on Ignition(%) 6.0 %
SiO2 50 %
ZrO2 10 %
 
Descriptive Properties
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Kaowool Millboard 822 Thermal Ceramic
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Morgan Advanced Ceramics Cerachrome® Refractory Ceramic Fiber Bulks Thermal Ceramic

CMORF7060 / 203359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.