MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Polytron® 79837 Vinyl Compound - Rigid (RPVC)  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Description/Features:

  • Interior
  • Static Dissipative
  • UL 94 V0
  • UL 94 V1

Applications:

  • Custom Profiles

Processing Method:

  • Extrusion-Sheet
  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Recommend drying material for a minimum of 2 hours at 160 degrees Fahrenheit.
Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78.715 sec; ASTM D2240
Tensile Strength, Yield 6100 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 323000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 9894 psiASTM D790
Flexural Modulus 316 ksiASTM D790
Izod Impact, Notched 6.30 ft-lb/in
@Thickness 3.17 mm
Method A, With Grain - Comp. Molded; ASTM D256
 8.10 ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
Method A, Against Grain - Comp. Molded; ASTM D256
Dart Drop Total Energy 0.100 ft-lb/milProcedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
 0.390 ft-lb/milProcedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmASTM D257
Surface Resistivity per Square 1.00e+11 ohmASTM D257
Static Decay 2.0 sec5,000 to 0 volts, 15 %
 2.0 sec5,000 to 0 volts, 50 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 47.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 158 °FUnannealed, 0.125 in bars; ASTM D648
Flammability, UL94 V-1Natural
 V-0All Colors
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 380 °FExtrusion
 
Descriptive Properties
Cell Classification D178414324ASTM D1784
Ease of SizingAcceptable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 3121 Rigid PVC, Extrusion
Axiall 7555 Rigid PVC, Extrusion, White
Axiall 5006 Rigid PVC, Extrusion, White
Axiall 3101 Rigid PVC, Extrusion
Geon® Performance Solutions x150-206-14702 Vinyl Compound - Rigid (RPVC)

PH1PO3072 / 44876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.