MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).

Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and elasticity.

Uses: Blown and flat die/cast film extrusion, injection molding and cable jacketing.

Complies with FDA 177.1680 and FDA 177.2600

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccASTM D792
Water Vapor Transmission 420 g/m²/dayASTM E96B
 3200 g/m²/dayASTM D6701
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70
@Time 5.00 sec
ASTM D2240
Tensile Strength, Ultimate 5300 psiASTM D412
Elongation at Break 730 %ASTM D412
100% Modulus 0.00340 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.00550 GPa
@Strain 300 %
ASTM D412
Tear Strength 110 pliTrouser; ASTM D470
Graves Tear Strength 380 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 17
@Load 1.00 kg
H-18 wheel; ASTM D3389
Tensile Set 6.0 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °CDSC
 150 °CKofler
Glass Transition Temp, Tg -70.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Zone 1 171 °CExtrusion
Zone 2 177 °CExtrusion
Zone 3 182 °CExtrusion
Zone 4 188 °CExtrusion
Adapter Temperature 193 °C5, Extrusion
Die Temperature 193 °C6, Zone 1, Extrusion
 193 °CZone 2, Extrusion
Drying Temperature 82.0 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU

PNOVEON592 / 121483

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.