Specifically designed for use in injection molded food serviceware applications. This opaque, off-white molding grade creates parts that are rigid and heat resistant for tableware used with hot foods and drinks when injection molded using conventional chilled molds. Ingeo AW 300D is fully formulated to be used naturally, but may be blended with color compounds.Information provided by NatureWorks LLC. |