MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell Solstice® Gas Blowing Agent
Categories: Fluid

Material Notes:
  • High insulation performance
  • Low GWP of <1
  • Non-flammable and safe to use
  • Low rate of diffusion and longer insulation life
  • Low transition costs to convert from HFC and non-fluorocarbon blowing agents
Honeywell Solstice® Gas Blowing Agent (GBA) has been developed for extruded polystyrene, and pressurized one- and two-component PUR foams. It is a replacement for HFC-134a and other fluorocarbon and non-fluorocarbon blowing agents. Solstice GBA is non-flammable having a boiling point of -3°F. It has an ultra low GWP of <1, a low MIR, low POCP and low contribution to ground level smog formation. Solstice GBA allows extrusion of thick, dimensionally stable foam. XPS boards produced using Solstice GBA have achieved lambda values as low as 27mW/m•K as per EN 13164 Annex C. Solstice GBA is a near drop-in replacement for many extrusion processes currently using CO2, HFC-134a and HFC-152a blowing agents.

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 114 g/mol
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0130 W/m-KVapor
Boiling Point -3.00 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitemp AF2-IDA6 Nickel Alloy
Unitemp® AF2-IDA Nickel Alloy
Evonik Butene-1 Combustible gas
Novatec Novablend® 8829 PVC
MAR-M432 Cast Nickel Superalloy

PHONWL169 / 179714

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.