MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unitemp AF2-IDA6 Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.26 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1290 MPa
@Temperature 760 °C
187000 psi
@Temperature 1400 °F
Bar
 1400 MPa
@Temperature 650 °C
203000 psi
@Temperature 1200 °F
Bar
 1480 MPa
@Temperature 540 °C
215000 psi
@Temperature 1000 °F
Bar
 1560 MPa
@Temperature 21.0 °C
226000 psi
@Temperature 69.8 °F
Bar
Tensile Strength, Yield  995 MPa
@Strain 0.2 %,
Temperature 760 °C
144000 psi
@Strain 0.2 %,
Temperature 1400 °F
Bar
 1015 MPa
@Strain 0.2 %,
Temperature 21.0 °C
147200 psi
@Strain 0.2 %,
Temperature 69.8 °F
Bar
 1020 MPa
@Strain 0.2 %,
Temperature 650 °C
148000 psi
@Strain 0.2 %,
Temperature 1200 °F
Bar
 1040 MPa
@Strain 0.2 %,
Temperature 540 °C
151000 psi
@Strain 0.2 %,
Temperature 1000 °F
Bar
Elongation at Break  16 %
@Temperature 760 °C
16 %
@Temperature 1400 °F
Bar
 18 %
@Temperature 650 °C
18 %
@Temperature 1200 °F
Bar
 19 %
@Temperature 540 °C
19 %
@Temperature 1000 °F
Bar
 20 %
@Temperature 21.0 °C
20 %
@Temperature 69.8 °F
Bar
Rupture Strength  360 MPa
@Temperature 760 °C,
Time 3.60e+6 sec
52200 psi
@Temperature 1400 °F,
Time 1000 hour
Bar
 885 MPa
@Temperature 650 °C,
Time 3.60e+6 sec
128000 psi
@Temperature 1200 °F,
Time 1000 hour
Bar
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 4.0 %4.0 %
Boron, B 0.015 %0.015 %
Carbon, C 0.040 %0.040 %
Chromium, Cr 12 %12 %
Cobalt, Co 10 %10 %
Molybdenum, Mo 2.7 %2.7 %
Nickel, Ni 60 %60 %
Titanium, Ti 2.8 %2.8 %
Tungsten, W 6.5 %6.5 %
Zirconium, Zr 0.10 %0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell Solstice® Gas Blowing Agent
Unitemp® AF2-IDA Nickel Alloy
Special Metals Udimet® 700 Nickel Alloy
Special Metals Udimet® 710 Nickel Alloy
MAR-M432 Cast Nickel Superalloy

NZ986 / 170615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.