MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unitemp AF2-IDA6 Nickel Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.26 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1290 MPa
@Temperature 760 °C
Bar
 1400 MPa
@Temperature 650 °C
Bar
 1480 MPa
@Temperature 540 °C
Bar
 1560 MPa
@Temperature 21.0 °C
Bar
Tensile Strength, Yield 995 MPa
@Strain 0.2 %,
Temperature 760 °C
Bar
 1015 MPa
@Strain 0.2 %,
Temperature 21.0 °C
Bar
 1020 MPa
@Strain 0.2 %,
Temperature 650 °C
Bar
 1040 MPa
@Strain 0.2 %,
Temperature 540 °C
Bar
Elongation at Break 16 %
@Temperature 760 °C
Bar
 18 %
@Temperature 650 °C
Bar
 19 %
@Temperature 540 °C
Bar
 20 %
@Temperature 21.0 °C
Bar
Rupture Strength 360 MPa
@Temperature 760 °C,
Time 3.60e+6 sec
Bar
 885 MPa
@Temperature 650 °C,
Time 3.60e+6 sec
Bar
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 %
Boron, B 0.015 %
Carbon, C 0.040 %
Chromium, Cr 12 %
Cobalt, Co 10 %
Molybdenum, Mo 2.7 %
Nickel, Ni 60 %
Titanium, Ti 2.8 %
Tungsten, W 6.5 %
Zirconium, Zr 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell Solstice® Gas Blowing Agent
Unitemp® AF2-IDA Nickel Alloy
Special Metals Udimet® 700 Nickel Alloy
Special Metals Udimet® 710 Nickel Alloy
MAR-M432 Cast Nickel Superalloy

NZ986 / 170615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.