MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 33% glass-fiber, impact modified
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D792
Density 1.50 g/cc0.0542 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 294-4
 0.0050 cm/cm0.0050 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inISO 294-4
Melt Flow 7.0 g/10 min7.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7171ISO 2039-2
Tensile Strength at Break 110 MPa16000 psi5mm/min; ISO 527-2/1A
 110 MPa
@Temperature 22.8 °C
16000 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527-2/1A
 4.0 %
@Temperature 22.8 °C
4.0 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 9.50 GPa1380 ksi1mm/min; ISO 527-2/1A
Flexural Strength 170 MPa24700 psiISO 178
 172 MPa
@Temperature 22.8 °C
25000 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 9.00 GPa1310 ksiISO 178
 8.27 GPa
@Temperature 22.8 °C
1200 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 1.33 J/cm
@Temperature 22.8 °C
2.50 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO) 13.2 kJ/m²6.28 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 5.40 J/cm²25.7 ft-lb/in²ISO 179/1eU
 5.40 J/cm²
@Temperature -30.0 °C
25.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.31 J/cm²6.23 ft-lb/in²ISO 179/1eA
 1.32 J/cm²
@Temperature -30.0 °C
6.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 60093
Dielectric Strength 21.7 kV/mm550 kV/inshort term; ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C36.1 µin/in-°FISO 11359-2
Melting Point 225 °C437 °FISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 223 °C433 °FASTM D648
 224 °C435 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 206 °C403 °FISO 75-1, -2
 209 °C408 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °Fhopper
 65.0 - 93.0 °C149 - 199 °Fcavity
Feed Temperature 230 - 240 °C446 - 464 °F
Zone 1 230 - 240 °C446 - 464 °F
Zone 2 235 - 250 °C455 - 482 °F
Zone 3 235 - 250 °C455 - 482 °F
Zone 4 240 - 260 °C464 - 500 °F
Die Temperature 250 - 260 °C482 - 500 °F
Melt Temperature 235 - 260 °C455 - 500 °F
 260 °C500 °FISO 294
Mold Temperature 82.0 °C180 °FISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Necessary low maximum
Injection Pressure 48.0 MPa6960 psiISO 294
Hot-Working Temperature 250 - 260 °C482 - 500 °F
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Melt volume rate (MVR), cm³/10min5.7
MVR test load, kg2.16
MVR test temperature, °C250
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced

PHCS074 / 123489

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.