MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Celanex® 4305 PBT, 33% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Celanex 4305 is a 33% glass reinforced, toughened, thermoplastic polyester.
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 33% glass-fiber, impact modified
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/ccASTM D792
Density 1.50 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cmISO 294-4
 0.0050 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cmISO 294-4
Melt Flow 7.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 71ISO 2039-2
Tensile Strength at Break 110 MPa5mm/min; ISO 527-2/1A
 16000 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 3.0 %5mm/min; ISO 527-2/1A
 4.0 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 9500 MPa1mm/min; ISO 527-2/1A
Flexural Strength 170 MPaISO 178
 25000 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 9000 MPaISO 178
 1.20e+6 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 2.50 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Izod Impact, Notched (ISO) 13.2 kJ/m²ISO 180/1A
Charpy Impact Unnotched 54.0 kJ/m²ISO 179/1eU
 54.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 13.1 kJ/m²ISO 179/1eA
 13.2 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Strength 550 V/milshort term; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 65.0 µm/m-°CISO 11359-2
Melting Point 225 °CISO 11357-1,-2,-3
 437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 224 °CISO 75-1, -2
 433 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °CISO 75-1, -2
 408 °FASTM D648
Flammability, UL94 HB
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 50.0 °Chopper
 65.0 - 93.0 °Ccavity
Feed Temperature 230 - 240 °C
Zone 1 230 - 240 °C
Zone 2 235 - 250 °C
Zone 3 235 - 250 °C
Zone 4 240 - 260 °C
Die Temperature 250 - 260 °C
Melt Temperature 235 - 260 °C
 260 °CISO 294
Mold Temperature 82.0 °CISO 294
Injection Velocity 300 mm/secISO 294
Drying Temperature 120 - 130 °C
Dry Time 4 hour
Moisture Content 0.020 %Necessary low maximum
Injection Pressure 48.0 MPaISO 294
Hot-Working Temperature 250 - 260 °C
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Melt volume rate (MVR), cm³/10min5.7
MVR test load, kg2.16
MVR test temperature, °C250
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celanex® 5300-2UV PBT, 30% Glass Reinforced

PHCS074 / 123489

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.