MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotchkote™ 175UC Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Coating 175UC has been specifically developed as a 100% solids

Product Features:

  • Combines good application characteristics with excellent corrosion protection and ultimate chemical resistance.
  • Is designed for application in two or more coats by brush or roller
  • Is primarily intended fro use on steel but can also by used on concrete surfaces with the appropriate primer.
  • Adhesion-Excellent to surfaces prepared as recommended.
  • Corrosion Resistance-Excellent resistance to abrasion and mechanical damage.
  • Chemical Resistance-Suitable for continuous immersion in inorganic acids.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cc
Solids Content 100 %
Thickness 10.0 mil
 
Processing PropertiesOriginal ValueComments
Cure Time 4.50 hourFull Cure
 168 hourTouch Dry
 
Descriptive Properties
AppearanceLight and Dark Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotchkote™ 175SR Epoxy Coating
3M Scotchkote™ 162HB Epoxy Coating

PMM35284 / 170031

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.