MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M Scotchkote™ 162HB Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw water, and effluent. The product can also be used on externals of pipes where an abrasion-resistant system is required. This material is designed for application in a single high build coat of up to 1mm, by plural feed hot airless spray and can be used on both steel and concrete surfaces.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³
Solids Content 100 %100 %
Volatile Organic Compounds (VOC) Content 6.5 g/l6.5 g/l
Water Absorption 0.72 %0.72 %21 days; ASTM D570
Water Vapor Transmission 1.20 g/m²/day0.0773 g/100 in²/dayASTM D1653
Oxygen Transmission Rate 0.947 cc/m²/day0.0610 cc/100 in²/dayASTM D3958
Thickness 508 microns20.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D2240
Tensile Strength at Break 24.0 MPa3480 psiASTM D638
Elongation at Break 1.4 %1.4 %ASTM D638
Flexural Strength 52.0 MPa7540 psiASTM D790
Impact Test 8.00 J5.90 ft-lb1/8" steel plate; ASTM G14 (modified)
Abrasion 105105[mg] CS-17, 1000 cycles; ASTM D4060
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.7 kV/mm400 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 26.0 °C78.8 °F
 56.0 °C133 °Fonset
 
Processing PropertiesMetricEnglishComments
Cure Time 360 min6.00 hourTouch Dry
 960 min16.0 hourHard Dry
 10100 min168 hourFull Cure
 
Descriptive Properties
AppearanceGray and Red Oxide
Pencil Hardness2HASTM D3363

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating
Chesterton ARC 10 Paste grade machinable composite
3M Scotchkote™ HTX 517 Epoxy HT Lining
3M Scotchkote™ 175UC Epoxy Coating
3M Scotchkote™ 175SR Epoxy Coating

PMM35337 / 170084

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.