MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8202C PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique crystalline structure results in increased strength, stiffness, heat distortion temperature and performance under load as a homopolymer. It also cycles faster while maintaining properties and resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Water Absorption 1.6 %24 hour; ISO Test
 9.3 %ISO 62
Moisture Absorption at Equilibrium 2.6 %23°C/50% R.H.; ISO 62
Relative Viscosity 2.6 cPISO Test; 96 % SAV
Viscosity Measurement 48Formic Acid
Linear Mold Shrinkage 0.0090 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM Test
Tensile Strength at Break 90.0 MPa0.2 in/min; ASTM Test
 25.0 MPa
@Temperature 120 °C
ASTM Test
 25.0 MPa
@Temperature 120 °C
ISO Data
 35.0 MPa
@Temperature 80.0 °C
ISO Data
 35.0 MPa
@Temperature 80.0 °C
ASTM Test
 130 MPa
@Temperature -40.0 °C
ASTM Test
 130 MPa
@Temperature -40.0 °C
ISO Data
Tensile Strength, Yield 88.0 MPa50mm/min; ISO 527
 90.0 MPa2 in/min; ASTM Test
 30.0 MPa
@Temperature 120 °C
ASTM Test
 30.0 MPa
@Temperature 120 °C
ISO Data
 40.0 MPa
@Temperature 80.0 °C
ISO Data
 40.0 MPa
@Temperature 80.0 °C
ASTM Test
 137 MPa
@Temperature -40.0 °C
ASTM Test
 137 MPa
@Temperature -40.0 °C
ISO Data
Elongation at Break 7.0 %50mm/min, Nominal strain; ISO 527
 12 %2 in/min; ASTM Test
 >= 100 %
 5.0 %
@Temperature -40.0 °C
ASTM Test
 5.0 %
@Temperature -40.0 °C
ISO Data
 >= 100 %
@Temperature 120 °C
ISO Data
 >= 100 %
@Temperature 80.0 °C
ISO Data
 >= 100 %
@Temperature 120 °C
ASTM Test
Elongation at Yield 4.0 %50mm/min; ISO 527
 4.0 %2 in/min; ASTM Test
 3.0 %
@Temperature -40.0 °C
ASTM Test
 3.0 %
@Temperature -40.0 °C
ISO Data
 25 %
@Temperature 80.0 °C
ASTM Test
 25 %
@Temperature 80.0 °C
ISO Data
 27 %
@Temperature 120 °C
ASTM Test
 27 %
@Temperature 120 °C
ISO Data
Tensile Modulus 3700 MPa1mm/min; ISO 527
 550 MPa
@Temperature 120 °C
ISO Data
 750 MPa
@Temperature 80.0 °C
ISO Data
 4090 MPa
@Temperature -40.0 °C
ISO Data
Flexural Strength 95.0 MPaISO Data
 110 MPaASTM Test
 21.0 MPa
@Temperature 120 °C
ASTM Test
 30.0 MPa
@Temperature 65.0 °C
ASTM Test
 183 MPa
@Temperature -40.0 °C
ASTM Test
Flexural Modulus 2800 MPaISO Data
 3170 MPaASTM Test
 385 MPa
@Temperature 120 °C
ASTM Test
 440 MPa
@Temperature 93.0 °C
ASTM Test
 600 MPa
@Temperature 65.0 °C
ASTM Test
Izod Impact, Notched 0.320 J/cm
@Temperature -40.0 °C
ASTM Test
 0.480 J/cm
@Thickness 3.17 mm
ASTM Test
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 0.350 J/cm²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 81.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM Test
Melting Point 220 °C10 K/min
 220 °CASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 165 °CISO 75
 190 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CISO 75
 75.0 °CASTM Test
Flammability, UL94 V-2
@Thickness 0.700 mm
 V-2
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °CInjection molding
Mold Temperature 80.0 °CInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedNo
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8202C PA6 (Conditioned)
BASF Ultramid® A3K PA66 (Dry)
BASF Ultramid® 8202 PA6 (Dry)
BASF Ultramid® 8253 HS PA6 (Dry)
Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)

PBASF9145 / 84909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.