MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes:

These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended to jet melt completely and to clean the cylinder, e.g. with a standard polyamide.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³±0.03 g/cm³; DIN 53479
Filler Content 15 %15 %Glass Fiber Reinforcement
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa
@Temperature 23.0 °C
15200 psi
@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 7.00 GPa
@Temperature 23.0 °C
1020 ksi
@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmIEC 60093
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 261 °C502 °FISO 3146
UL RTI, Electrical  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746
 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 100 °C
@Thickness 0.750 mm
212 °F
@Thickness 0.0295 in
UL 746
 110 °C
@Thickness 1.50 mm
230 °F
@Thickness 0.0591 in
UL 746
 120 °C
@Thickness 3.00 mm
248 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.400 mm
149 °F
@Thickness 0.0157 in
UL 746
 105 °C
@Thickness 0.750 mm
221 °F
@Thickness 0.0295 in
UL 746
 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
ALL; UL 94
 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
ALL; UL 94
 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
ALL; Internal Method
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
ALL; UL 94
Glow Wire Ignition Temperature  960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-13
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °FDesiccant Dryer
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourDesiccant Dryer
Hold Pressure 40.0 - 90.0 MPa5800 - 13100 psi
 
Descriptive Properties
AdditiveHeat Stabilizer
Comparative Tracking Index (CTI)PLC 0UL 746; 3.00 mm
FeaturesFlame Retardant
 Halogen Free
 Heat Stabilized
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
RoHS ComplianceRoHS Compliant
UL File NumberE76261

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8202C PA6 (Dry)
Mitsubishi Xantar® FC 23 UR Polycarbonate
LG Chemical Lupox® GP1006FD PBT
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Covestro Makrolon® 6487 Polycarbonate, Flame Retardant Grade

PH0POL0774 / 145343

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.