MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Afton Plastics 2400 40% Glass Filled Polyetherimide
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 40% Glass Fiber

Material Notes: Afton plastics produces shapes and components from SABIC Ultem® 240 PEI, a high performance material that exhibits high strength and heat resistant properties. Glass-filled grades provide improved rigidity and dimensional stability.

Product Benefits: UL 94 V-0 rating,• Microwave transparency • Temperature range: -4°F to +340°F • Withstands EtO, gamma radiation, autoclaving, and dry heat sterilization • Stable dielectric strength • Low thermal expansion • Low creep • Excellent hydrolytic and chemical stability.

Applications: Fluid handling components, • Medical trays and instruments • Photographic lens housing • High heat test fixtures • Glass reinforced for high stiffness electrical housings • Aircraft and automotive parts • Food processing manifolds.

Information provided by Afton Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.61 g/ccASTM D792
Water Absorption 0.13 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Tensile Strength at Break 25900 psiType 1, 0.2 in/min; ASTM D638
Elongation at Break 2.5 %Type 1, 0.2 in/min; ASTM D638
Flexural Strength 34900 psi0.1 in/min; ASTM D790
Flexural Modulus 1.699e+6 psi0.1 in/min; ASTM D790
Izod Impact, Notched 2.10 ft-lb/in
@Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.50e+16 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 610 V/mil
@Thickness 62.0 mm
In oil; ASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
Arc Resistance 120 - 180 sectungsten
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.00 µin/in-°F
@Temperature -17.8 - 149 °C
ASTM E831
Maximum Service Temperature, Air 340 °F
Deflection Temperature at 0.46 MPa (66 psi) 216 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °Cunannealed; ASTM D648
Vicat Softening Point 234 °CRate B/50; ASTM D1525
Minimum Service Temperature, Air -4.00 °F
Flammability, UL94 V-0
@Thickness 0.254 - 0.406 mm
Oxygen Index >= 54 %ASTM D2863

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 2102 Polyetherimide (PEI), Glass Fiber
RTP Company RTP 2100 TFE 5  Polyetherimide (PEI) PTFE 5%
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
Overview of materials for Nylon 66, Unreinforced
Lubrizol LifeSciences Isoplast® 2540 ETPU

PAFTON912 / 232137

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.