MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 40% Glass Fiber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.59 - 1.61 g/cc0.0574 - 0.0582 lb/in³Average value: 1.60 g/cc Grade Count:8
Filler Content 40.0 %40.0 %Average value: 40.0 % Grade Count:4
Water Absorption 0.130 - 0.180 %0.130 - 0.180 %Average value: 0.155 % Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.00350 cm/cm0.00100 - 0.00350 in/inAverage value: 0.00172 cm/cm Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114 - 123114 - 123Average value: 121 Grade Count:4
Tensile Strength, Ultimate 177 - 200 MPa25600 - 29000 psiAverage value: 184 MPa Grade Count:8
Tensile Strength, Yield 177 - 186 MPa25600 - 27000 psiAverage value: 180 MPa Grade Count:4
Elongation at Break 1.40 - 3.00 %1.40 - 3.00 %Average value: 2.22 % Grade Count:9
Modulus of Elasticity 10.3 - 15.2 GPa1500 - 2200 ksiAverage value: 13.0 GPa Grade Count:7
Flexural Yield Strength 234 - 283 MPa33900 - 41000 psiAverage value: 251 MPa Grade Count:9
Flexural Modulus 11.0 - 15.2 GPa1600 - 2200 ksiAverage value: 12.1 GPa Grade Count:9
Compressive Yield Strength 155 - 169 MPa22500 - 24500 psiAverage value: 164 MPa Grade Count:3
Izod Impact, Notched 0.960 - 1.12 J/cm1.80 - 2.10 ft-lb/inAverage value: 1.00 J/cm Grade Count:8
Izod Impact, Unnotched 4.27 - 6.94 J/cm8.00 - 13.0 ft-lb/inAverage value: 6.10 J/cm Grade Count:5
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+12 - 1.50e+16 ohm-cm1.00e+12 - 1.50e+16 ohm-cmAverage value: 6.68e+15 ohm-cm Grade Count:6
Dielectric Constant 3.70 - 4.003.70 - 4.00Average value: 3.88 Grade Count:5
Dielectric Strength 19.7 - 24.0 kV/mm500 - 610 kV/inAverage value: 21.3 kV/mm Grade Count:5
Dissipation Factor 0.00200 - 0.005000.00200 - 0.00500Average value: 0.00380 Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.4 - 21.6 µm/m-°C8.00 - 12.0 µin/in-°FAverage value: 18.0 µm/m-°C Grade Count:5
Thermal Conductivity 0.259 W/m-K1.80 BTU-in/hr-ft²-°FAverage value: 0.259 W/m-K Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 210 - 216 °C410 - 421 °FAverage value: 213 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 207 - 213 °C405 - 415 °FAverage value: 210 °C Grade Count:8
Vicat Softening Point 232 - 234 °C450 - 453 °FAverage value: 233 °C Grade Count:3
Flammability, UL94 V-0V-0Grade Count:6
 
Processing PropertiesMetricEnglishComments
Melt Temperature 107 - 399 °C225 - 750 °FAverage value: 350 °C Grade Count:5
Mold Temperature 107 - 399 °C225 - 750 °FAverage value: 186 °C Grade Count:6
Drying Temperature 138 - 149 °C280 - 300 °FAverage value: 146 °C Grade Count:5
Moisture Content 0.0400 %0.0400 %Average value: 0.0400 % Grade Count:3
Injection Pressure 82.7 - 124 MPa12000 - 18000 psiAverage value: 103 MPa Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI)
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled

O3614 / 78228

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.